Inter J Stomatol ›› 2016, Vol. 43 ›› Issue (2): 165-167.doi: 10.7518/gjkq.2016.02.011

Previous Articles     Next Articles

Effect of polishing and glazing techniques on the wearing of zirconia crown against enamel

Chen Jifen1, Ding Hong2   

  1. 1. Dept. of Prosthodontics, Dalian Stomatological Hospital, Dalian 116021, China; 2. Dept. of Comprehensive Dentistry, Dalian Stomatological Hospital, Dalian 116021, China)
  • Received:2015-09-17 Revised:2015-12-15 Online:2016-03-01 Published:2016-03-01

Abstract: Objective This in vitro study aimed to measure the roughness and wearing of polished, glazed, and polished and then reglazed zirconia against human enamel antagonists. Methods Zirconia specimens were divided into the polished, glazed, and polished and then reglazed groups(n=8). Enamel was used as a control. The mesiobuccal cusps of extracted maxillary third molars were standardized and used as antagonists. The surface roughness of all pretest specimens was measured, and the effects of treated zirconia on the wear property of the enamel were evaluated by a wear test. Results Surface roughness increased in the following order: polished zirconia

Key words: zirconia, polish, wear, glaze, zirconia, polish, wear, glaze

CLC Number: 

  • R 783.1

TrendMD: 
[1] Conrad HJ, Seong WJ, Pesun IJ. Current ceramic materials and systems with clinical recommendations: a systematic review[J]. J Prosthet Dent, 2007, 98(5):389-404.
[2] Guess PC, Schultheis S, Bonfante EA, et al. Allceramic systems: laboratory and clinical performance [J]. Dent Clin North Am, 2011, 55(2):333-352.
[3] Nakamura Y, Hojo S, Sato H. The effect of surface roughness on the Weibull distribution of porcelain strength[J]. Dent Mater J, 2010, 29(1):30-34.
[4] Passos SP, de Freitas AP, Iorgovan G, et al. Enamel wear opposing different surface conditions of different CAD/CAM ceramics[J]. Quintessence Int, 2013, 44(10):743-751.
[5] Elmaria A, Goldstein G, Vijayaraghavan T, et al. An evaluation of wear when enamel is opposed by various ceramic materials and gold[J]. J Prosthet Dent, 2006, 96(5):345-353.
[6] Oh WS, Delong R, Anusavice KJ. Factors affecting enamel and ceramic wear: a literature review[J]. J Prosthet Dent, 2002, 87(4):451-459.
[7] Heintze SD, Cavalleri A, Forjanic M, et al. Wear of ceramic and antagonist—a systematic evaluation of influencing factors in vitro[J]. Dent Mater, 2008, 24(4):433-449.
[8] Etman MK. Confocal examination of subsurface cracking in ceramic materials[J]. J Prosthodont, 2009, 18(7):550-559.
(本文采编 王晴)
[1] Wang Xiao-chen,Wang Jian.. Research progress on preparation forms for the margin of monolithic zirconia crowns in posterior teeth [J]. Int J Stomatol, 2023, 50(4): 485-490.
[2] Zeng Fang,Wang Jian. Influencing factors of aesthetic prosthesis performance of monolithic zirconia crowns [J]. Int J Stomatol, 2022, 49(2): 233-238.
[3] Yang Guangmei,Wang Jian. Mechanical properties of monolithic zirconia crowns and its relationship with clinical application [J]. Int J Stomatol, 2022, 49(1): 79-84.
[4] Li Min,Hua Chengge,Jiang Li. Research progress on new technology for improving adhesion properties of zirconia ceramics [J]. Int J Stomatol, 2021, 48(4): 485-490.
[5] Wan Qianbing. My opinion on the generations of dental zirconia materials [J]. Int J Stomatol, 2021, 48(2): 125-128.
[6] Qing Ping,Gao Shanshan,Qian Linmao,Yu Haiyang. Microtribological behaviour of human tooth enamel treated by gamma irradiation [J]. Int J Stomatol, 2020, 47(2): 189-195.
[7] Wan Qianbing. Research status and clinical outcomes of zirconia abutments [J]. Inter J Stomatol, 2018, 45(1): 1-8.
[8] Wan Qianbing. Several problems on monolithic zirconia crowns [J]. Inter J Stomatol, 2018, 45(1): 9-13.
[9] Zhang Yarong, Liu Yang, Zhang Ling, Yu Haiyang. Quantitative analysis of the load tolerance of maxillary incisors with ceramic-laminated veneers for various incisal margin preparations [J]. Inter J Stomatol, 2017, 44(3): 301-303.
[10] Yao Chenmin, Zhou Liqun, Huang Cui.. Selection of tooth-colored restorative material for worn anterior teeth [J]. Inter J Stomatol, 2017, 44(3): 363-367.
[11] Yang Yun, Li Zhen, Meng Xiangfeng, Qian Dongdong.. Treating severe tooth wear through occlusal reconstruction [J]. Inter J Stomatol, 2017, 44(2): 148-152.
[12] Lin Jie1, Zheng Zhifeng2, Lu Zhaojie1, Li Xiurong2, Zheng Zhiqiang1.. Design and bonding technique of posterior zirconia resin-bonded fixed partial dentures [J]. Inter J Stomatol, 2015, 42(6): 624-627.
[13] Wang Wanwei, Chen Yuanhua, Yu Qing. Relationship between colorimetry and transparency of zirconia ceramic with clinical all-ceramic crown repair [J]. Inter J Stomatol, 2015, 42(3): 302-305.
[14] Du Qiao, Niu Guangliang. Surface roughening zirconia and modification [J]. Inter J Stomatol, 2015, 42(1): 97-101.
[15] Sun Changjuan, Guan Hongyu, Han Lu. Clinical effects of an in-office desensitizing polishing paste containing arginine and calcium carbonate on root-dentin hypersensitivity after subgingival scaling with ultrasonic instruments [J]. Inter J Stomatol, 2014, 41(6): 663-666.
Viewed
Full text


Abstract

Cited

  Shared   
  Discussed   
[1] . [J]. Foreign Med Sci: Stomatol, 1999, 26(06): .
[2] . [J]. Foreign Med Sci: Stomatol, 1999, 26(06): .
[3] . [J]. Foreign Med Sci: Stomatol, 1999, 26(06): .
[4] . [J]. Foreign Med Sci: Stomatol, 1999, 26(06): .
[5] . [J]. Foreign Med Sci: Stomatol, 1999, 26(06): .
[6] . [J]. Foreign Med Sci: Stomatol, 1999, 26(05): .
[7] . [J]. Foreign Med Sci: Stomatol, 1999, 26(05): .
[8] . [J]. Foreign Med Sci: Stomatol, 1999, 26(05): .
[9] . [J]. Foreign Med Sci: Stomatol, 1999, 26(04): .
[10] . [J]. Foreign Med Sci: Stomatol, 1999, 26(04): .