两种镍基口腔修复合金在漱口水中镍离子析出的比较

田陶然,张扬根,黄鑫琪,李龙飚,张心曦,朱卓立   

  1. 口腔疾病研究国家重点实验室 华西口腔医院(四川大学) 成都 610041
  • 收稿日期:2015-12-01 修回日期:2016-02-13 出版日期:2016-05-01 发布日期:2016-05-01
  • 通讯作者: 朱卓立,讲师,博士,Email:zzl7505@126.com
  • 作者简介:田陶然,硕士,Email:tiantrcd@163.com
  • 基金资助:
    四川省医学会科研课题(S15061)

Comparative study on nickel release of two dental nickel alloys in mouth wash

Tian Taoran, Zhang Yanggen, Huang Xinqi, Li Longbiao, Zhang Xinxi, Zhu Zhuoli   

  1. State Key Laboratory of Oral Diseases, West China Hospital of Stomatology, Sichuan University, Chengdu 610041, China) This study was supported by the Science Foudation of Sichuan Medical Association(S15061).
  • Received:2015-12-01 Revised:2016-02-13 Online:2016-05-01 Published:2016-05-01

摘要: 目的 通过连续浸泡实验探究两种镍基口腔修复常用合金在漱口水中的镍离子析出情况。方法 将镍基铸造合金和镍铬烤瓷合金的标准试件逐级打磨后,放在分别由漱口水、蒸馏水和人工唾液配制的实验组和对照组溶液中,连续恒温(37±1)℃浸泡96 h后,使用电感耦合等离子体发射光谱仪(ICP-OES)测定溶液中析出的镍离子的量。结果 在没有金属浸泡的空白对照的实验组和对照组溶液中镍离子含量低于ICP-OES的检出限。在对照组溶液及实验组溶液中浸泡后镍基铸造合金组测得的镍离子析出均大于镍铬烤瓷合金组。两种金属试件在实验组溶液中的析出均大于在对照组溶液中的析出,差异明显。结论 漱口水对两种镍基合金中镍离子的析出均有促进作用,其中又以镍基铸造合金为甚。

关键词: 漱口水, 牙科合金, 浸渍, 镍, 漱口水, 牙科合金, 浸渍,

Abstract: Objective This study aims to investigate the release of nickel from two nickel alloy specimens for dental prosthesis in a commercial mouth wash through a constant immersion experiment. Methods Standard samples were casted from two different alloys and ground to achieve the same roughness. For our experimental group, one-half of the samples are immersed in a solution composed of artificial saliva and commercial mouthwash. For our control group, the other half of the samples are placed in a solution containing artificial saliva and distilled water. This procedure is performed at (37±1) °C for 96 h. The amount of Ni ion released after the 96 h immersion test and the changes in the surfaces of the alloys asreceived and upon immersion are then determined by using an inductively coupled plasma optical emission spectrometer(ICP-OES) and a scanning electron microscope. Results The amount of released Ni ion is below the minimum detection limit of ICP-OES in the blank solution without the alloys. More ions are released from the Ni-casted alloy than from the Ni-Cr porcelain fused to a metal in the experimental group and the control group. The ions released from each alloy are also significantly different in the two solutions. Conclusion The tested commercial mouthwash accelerates the release of Ni ion from the two nickel alloys. This phenomenon is more significant in the nickel-casted alloy than in the other alloy type.

Key words: mouth wash, dental alloy, immersion, nickel, mouth wash, dental alloy, immersion, nickel

中图分类号: 

  • R 783
[1] Wataha JC, Drury JL, Chung WO. Nickel alloys in the oral environment[J]. Expert Rev Med Devices, 2013, 10(4):519-539.
[2] Muris J, Goossens A, Gon?alo M, et al. Sensitization to palladium and nickel in Europe and the relationship with oral disease and dental alloys[J]. Contact Derm, 2015, 72(5):286-296.
[3] Büyük?ztürk S, Gelincik A, ünal D, et al. Oral nickel exposure may induce TypeⅠhypersensitivity reaction in nickel-sensitized subjects[J]. Int Immunopharmacol, 2015, 26(1):92-96.
[4] Pazzini CA, Marques LS, Ramos-Jorge ML, et al. Longitudinal assessment of periodontal status in patients with nickel allergy treated with conventional and nickel-free braces[J]. Angle Orthod, 2012, 82(4):653-657.
[5] Iijima M, Yuasa T, Endo K, et al. Corrosion behavior of ion implanted nickel-titanium orthodontic wire in fluoride mouth rinse solutions[J]. Dent Mater J, 2010, 29(1):53-58.
[6] Robin A, Meirelis JP. Influence of fluoride concentration and pH on corrosion behavior of Ti-6Al-4V and Ti-23Ta alloys in artificial saliva[J]. Mater Corrosion, 2007(3):173-180.
[7] Aung EE, Ueno M, Zaitsu T, et al. Effectiveness of three oral hygiene regimens on oral malodor reduction: a randomized clinical trial[J]. Trials, 2015, 16:31.
[8] Ragsdale SW. Nickel biochemistry[J]. Curr Opin Chem Biol, 1998, 2(2):208-215.
[9] Wataha JC, O’Dell NL, Singh BB, et al. Relating nickel-induced tissue inflammation to nickel release in vivo[J]. J Biomed Mater Res, 2001, 58(5):537-544.
[10] Elshahawy WM, Watanabe I, Kramer P. In vitro cytotoxicity evaluation of elemental ions released from different prosthodontic materials[J]. Dent Mater, 2009, 25(12):1551-1555.
[11] Thyssen JP, Menné T. Metal allergy—a review on exposures, penetration, genetics, prevalence, and clinical implications[J]. Chem Res Toxicol, 2010, 23(2):309-318.
[12] Loch J, ?ukaszczyk A, Augustyn-Pieni??ek J, et al. Electrochemical behaviour of Co-Cr and Ni-Cr dental alloys[J]. Solid State Phenomena, 2015(227):451-454.
[13] Esquivel-Upshaw JF, Dieng FY, Clark AE, et al. Surface degradation of dental ceramics as a function of environmental pH[J]. J Dent Res, 2013, 92(5):467-471.
[14] Mutlu-Sagesen L, Ergun G, Karabulut E. Ion release from metal-ceramic alloys in three different media[J]. Dent Mater J, 2011, 30(5):598-610.
[15] Benyahia H, Ebntouhami M, Forsal I, et al. Corrosion resistance of NiTi in fluoride and acid environments[J]. Int Orthod, 2009, 7(4):322-334.
[16] Knutson KJ, Berzins DW. Corrosion of orthodontic temporary anchorage devices[J]. Eur J Orthod, 2013, 35(4):500-506.
[1] 张麒麟,李军,李姝慧. 根管预备机用镍钛锉的研究进展[J]. 国际口腔医学杂志, 2022, 49(6): 663-669.
[2] 戢晓,景钫淇,李雅,薛晶. 根管预备顺序的数据模拟优化研究[J]. 国际口腔医学杂志, 2022, 49(1): 37-47.
[3] 王宏媛,何露,张茹,郑德强,李红. 热处理连续旋转镍钛锉对重度弯曲根管成形能力的比较研究[J]. 国际口腔医学杂志, 2021, 48(3): 297-304.
[4] 高洁,马锐,葛振林. 热激活镍钛弓丝矫治效率的系统评价[J]. 国际口腔医学杂志, 2019, 46(4): 393-399.
[5] 李宗莉, 彭彬. HyFlex、S3、K3XF以及ProTaper在树脂模拟根管中成形能力的比较研究[J]. 国际口腔医学杂志, 2017, 44(3): 256-260.
[6] 孙晓阳, 李霞. 镍钛再治疗器械去除根管充填材料的研究进展[J]. 国际口腔医学杂志, 2017, 44(3): 284-287.
[7] 杨殷杰, 侯本祥, 侯晓玫. R-相热处理镍钛根管锉的力学性能和根管预备成形能力[J]. 国际口腔医学杂志, 2017, 44(2): 189-194.
[8] 秦琨1 张东坡2. 不同材料烤瓷冠与金属冠磁共振成像伪影的比较[J]. 国际口腔医学杂志, 2016, 43(5): 507-510.
[9] 蔡静静 葛久禹. 不同介质对镍钛器械疲劳抗性的影响[J]. 国际口腔医学杂志, 2015, 42(6): 739-743.
[10] 朱玉婷 刘江峰 黄江勇 徐妍 李艳利 李晓星 陈秉勋. 控制记忆型镍钛锉HyFlex CM根管预备的临床效果分析[J]. 国际口腔医学杂志, 2014, 41(5): 521-525.
[11] 赵朋朋 秦宗长. 根管治疗与根管壁微裂[J]. 国际口腔医学杂志, 2014, 41(4): 478-482.
[12] 刘昭慧 凌均棨. 三维自调节根管预备锉[J]. 国际口腔医学杂志, 2014, 41(3): 320-323.
[13] 郭咏娟 刘奕. 正畸固定矫治器释放镍离子对机体的影响[J]. 国际口腔医学杂志, 2013, 40(6): 758-759.
[14] 唐颖 袁剑鸣 潘峰. 肩台瓷金瓷冠在前牙修复中的临床效果观察[J]. 国际口腔医学杂志, 2013, 40(4): 456-458.
[15] 刘思茗综述 胡涛审校. 新型镍钛器械Twisted Files的应用[J]. 国际口腔医学杂志, 2013, 40(2): 185-187.
Viewed
Full text


Abstract

Cited

  Shared   
  Discussed   
[1] 张新春. 桩冠修复与无髓牙的保护[J]. 国际口腔医学杂志, 1999, 26(06): .
[2] 王昆润. 长期单侧鼻呼吸对头颅发育有不利影响[J]. 国际口腔医学杂志, 1999, 26(05): .
[3] 彭国光. 颈淋巴清扫术中颈交感神经干的解剖变异[J]. 国际口腔医学杂志, 1999, 26(05): .
[4] 杨凯. 淋巴化疗的药物运载系统及其应用现状[J]. 国际口腔医学杂志, 1999, 26(05): .
[5] 康非吾. 种植义齿下部结构生物力学研究进展[J]. 国际口腔医学杂志, 1999, 26(05): .
[6] 柴枫. 可摘局部义齿用Co-Cr合金的激光焊接[J]. 国际口腔医学杂志, 1999, 26(04): .
[7] 孟姝,吴亚菲,杨禾. 伴放线放线杆菌产生的细胞致死膨胀毒素及其与牙周病的关系[J]. 国际口腔医学杂志, 2005, 32(06): 458 -460 .
[8] 费晓露,丁一,徐屹. 牙周可疑致病菌对口腔黏膜上皮的粘附和侵入[J]. 国际口腔医学杂志, 2005, 32(06): 452 -454 .
[9] 赵兴福,黄晓晶. 变形链球菌蛋白组学研究进展[J]. 国际口腔医学杂志, 2008, 35(S1): .
[10] 庞莉苹,姚江武. 抛光和上釉对陶瓷表面粗糙度、挠曲强度及磨损性能的影响[J]. 国际口腔医学杂志, 2008, 35(S1): .